After-sales Service: | More Than 5 Years |
---|---|
Warranty: | More Than 5 Years |
Certification: | CE, ISO |
Surface: | Smooth |
Application: | Transportation Project, Hydraulic Project, Geotechnical Project, Environmental Project |
Feature: | Puncture Resistance, Impact Resistance, Tear Resistance |
Proveedores con licencias comerciales verificadas
No. | El tema | Valor | ||||||||
0.70 | 0.75 | 1.00 | 1.25 | 1.50 | 2.00 | 2.50 | 3.00 | |||
1 | Min densidad,(g/cm3). | 0.940 | ||||||||
2 | Límite de fluencia (TD,MD), N/mm≥ | 10 | 11 | 15 | 18 | 22 | 29 | 37 | 44 | |
3 | Resistencia a la ruptura (TD,MD)N/mm≥ | 19 | 20 | 27 | 33 | 40 | 53 | 67 | 80 | |
4 | Elongación de rendimiento (TD,MD),%≥ | 12 | ||||||||
5 | El alargamiento de rotura (TD,MD)%≥ | 700 | ||||||||
6 | La fuerza de rotura de la media (TD,MD),N≥ | 87 | 93 | 125 | 156 | 187 | 249 | 311 | 374 | |
7 | La resistencia de punción,N≥ | 220 | 240 | 320 | 400 | 480 | 640 | 800 | 960. | |
8 | El estrés de la resistencia de crack ,h≥ | 300 | ||||||||
9 | El contenido de carbono negro ,% | 2.0~3.0 | ||||||||
10 | Negro de carbono dispersión | Nueve de 10 grad I o II, a menos de 1 si grad III | ||||||||
11 |
(OIT)Tiempo de inducción de oxidación, mín. | La OIT estándar≥100 | ||||||||
La OIT de alta presión≥400 | ||||||||||
12 | El envejecimiento de la estufa a 80ºC (estándar OIT conservan después de 90 días), %≥ | 55 |
Proveedores con licencias comerciales verificadas