Método de casting: | Fundición en Arena |
---|---|
Fundición Material Forma: | Metal |
Metal casting: | Hierro Fundido |
Casting Formulario Conde Uso: | Permanente |
Tratamiento De Superficies: | Pulido |
Rugosidad De La Superficie: | Ra0.05 |
Proveedores con licencias comerciales verificadas
Mechanical Property | Centrifugal Castings | Static Castings |
Hardness of Body | HSD50-80 | HSD40-75 |
Hardness of Neck | HSD35-48 | HSD-32-55 |
Tensile Srength of Core | >450MPa | >300Mpa |
Grade | Hardness (HSD) |
C | Si | Mn | Ni | Cr | Mo | Mg | P | S |
SGI | 40-55 | 3.2-3.7 | 1.0-2.5 | 0.5-1.0 | 0.2-0.6 | 0.2-0.6 | >0.04 | <0.2 | <0.03 | |
SGII | 55-70 | 3.2-3.7 | 1.2-205 | 0.5-1.0 | 0.2-0.6 | 0.2-0.6 | >0.04 | <0.2 | <0.03 | |
SGIV | 48-70 | 3.2-3.7 | 1.0-2.5 | 0.5-1.0 | 0.5-1.0 | 0.2-0.6 | 0.2-0.6 | >0.04 | <0.2 | <0.03 |
SGV | 48-70 | 3.2-3.7 | 1.0-2.5 | 0.5-1.0 | 1.0-3.0 | 0.3-1.2 | 0.2-0.8 | >0.04 | <0.2 | <0.03 |
SGVI | 42-52 | 2.9-3.5 | 1.5-2.4 | 0.4-0.8 | 1.0-2.5 | 0.1-0.5 | 0.4-0.8 | >0.04 | <0.2 | <0.03 |
SGVII | 55-75 | 2.9-3.5 | 1.5-2.4 | 0.4-0.8 | 2.5-.5 | 0.1-0.5 | 0.4-1.0 | >0.04 | <0.2 | <0.03 |
For roughing or finishing stands rolling mill of section mill, wire and rods, bars mills, finishing stands and back up rolls of strip and narrow strip mills
Proveedores con licencias comerciales verificadas